深冷处理对EH40极寒环境船用钢板的海水腐蚀性能影响
|
沈树阳 1, 王东胜 1, 孙士斌 2, 杨剔 2, 赵前进 2, 王鑫 2, 张亚飞 2, 常雪婷 1( )
|
Corrosion Behavior in Artificial Seawater of Subzero Treated EH40 Marine Steel Suitable for ExtremelyCold Environments
|
SHEN Shuyang 1, WANG Dongsheng 1, SUN Shibin 2, YANG Ti 2, ZHAO Qianjing 2, WANG Xin 2, ZHANG Yafei 2, CHANG Xueting 1( )
|
|
图10. 未经和经过-80 ℃深冷处理的EH40钢的腐蚀机理
|
Fig.10. Corrosion mechanisms of EH40 steel without (a) and with (b) -80 ℃ cooling treatment after corrosion for 72 h
|
|
|
|
|