316L和HR-2不锈钢在盐酸液膜环境中的钝化与点蚀
|
|
Passivation and Pitting of 316L and HR-2 Stainless Steel in Hydrochloric Acid Liquid Membrane Environment
|
|
图3. 316L和HR-2不锈钢在1 mol/L 90、70和60 ℃ HCl溶液中的电化学阻抗图 |
Fig.3. Electrochemical impedance diagram of 316L (a) and HR-2 (b) stainless steel 1 mol/L HCl solutions at 90, 70 and 60 ℃ |
![]() |