热轧AH36船板钢在室内仓储条件下的腐蚀行为研究
|
Corrosion Behavior of Hot-rolled AH36 Plate in Indoor Storage Environment
|
图6. AH36钢红色氧化皮在室内仓库存放不同时间的宏观腐蚀形貌 |
Fig.6. Optical images of red oxide scale of AH36 steel after exposured in indoor storage for 0 d (a), 13 d (b), 35 d (c), 69 d (d), 91 d (e), 119 d (f), 152 d (g) and 182 d (h) |
![]() |