电站用奥氏体耐热钢HR3C与Sanicro25在超临界水中的氧化特性
|
Oxidation Characteristics of Austenitic Heat-resistant Steel HR3C and Sanicro25 in Supercritical Water for Power Station
|
图2. HR3C钢在650和700 ℃超临界水中氧化不同时间后的表面形貌 |
Fig.2. Surface morphologies of HR3C steel oxidized in supercritical water at 650 ℃ (a, b) and 700 ℃ (c, d) for 200 h (a, c) and 1000 h (b, d) |
![]() |