深海低溶解氧环境下Al-Zn-In-Mg-Ti牺牲阳极性能研究
孙海静(), 覃明, 李琳
Performance of Al-Zn-In-Mg-Ti Sacrificial Anode in Simulated Low Dissolved Oxygen Deep Water Environment
SUN Haijing(), QIN Ming, LI Lin

图10. Al-Zn-In-Mg-Ti合金在两种溶解氧条件下浸泡168 h后微观腐蚀形貌

Fig.10. Microscopic morphologies of Al-Zn-In-Mg-Ti alloy immersed for 168 h in artificial seawaters containing SDO (a) and LDO (b), and the magrified images of areas I in Fig.10a (c) and II in Fig.10c (d)