纳米Al2O3改性SiBCN陶瓷高温粘接剂的制备与性能研究
|
Preparation and Properties of Ceramics Composed of Nano-Al2O3 and Polysiloxane-polyborosilicate-TiB2 Modified Polysilborazane as High Temperature Adhesive for SiC Based Ceramics
|
图6. PPPT和PPPTA在1000和1200 ℃空气中裂解2 h后的XRD谱 |
Fig.6. XRD patterns of the joints of PPPT (a) and PPPTA (b) after pyrolyzed at 1000 and 1200 ℃ in air for 2 h |
![]() |