固溶处理制度对挤压态Mg-Zn-Y-Nd镁合金在模拟体液中腐蚀和析氢行为的影响规律研究
郏义征1, 王保杰2, 赵明君2, 许道奎3()
Effect of Solid Solution Treatment on Corrosion and Hydrogen Evolution Behavior of an As-extruded Mg-Zn-Y-Nd Alloy in an Artificial Body Fluid
JIA Yizheng1, WANG Baojie2, ZHAO Mingjun2, XU Daokui3()

图5. 在Hank's溶液中经不同时间预浸泡处理后T4态Mg-6Zn-1.2Y-0.8Nd合金样品的表面腐蚀形貌及三维高低差照片

Fig.5. Surface corrosion morphologies and 3D images of the T4-treated Mg-6Zn-1.2Y-0.8Nd alloy before and after pre-immersion in Hank's solution for 4 h (a), 24 h (b) and 48 h (c)