20#钢在含饱和CO2的离子液体醇胺溶液中的腐蚀行为研究
贺三1(), 孙银娟2, 张志浩2, 成杰2, 邱云鹏1, 高超洋1
Corrosion Behavior of 20# Steel in Alkanolamine Solution Mixed with Ionic Liquid Containing Saturated CO2
HE San1(), SUN Yinjuan2, ZHANG Zhihao2, CHENG Jie2, QIU Yunpeng1, GAO Chaoyang1

图4. 20#钢在含不同浓度[Bmim]BF4的混合溶液中外层腐蚀产物膜的EDS分析结果

Fig.4. EDS results of the outer layers of corrosion product films formed on 20# steel during immersion in the mixed solutions with different concentrations of [Bmim]BF4: (a) area I in Fig.2a, (b) area II in Fig.2b, (c) area III in Fig.2c, (d) area IV in Fig.2d