TP110TS和P110钢在CO2注入井环空环境中应力腐蚀行为比较
李清1,2, 张德平1,2, 李晓荣3, 王薇4, 孙宝壮5(), 艾池1()
Comparison of Stress Corrosion Behavior of TP110TS and P110 Steel in a Simulated Annular Environment of CO2 Injection Well
LI Qing1,2, ZHANG Deping1,2, LI Xiaorong3, WANG Wei4, SUN Baozhuang5(), AI Chi1()

图3. P110和 TP110TS钢在不同浓度缓蚀剂条件下浸泡720 h除锈后的微观形貌

Fig.3. Micromorphologies of P110 (a~c) and TP110TS (d~f) steels after immersion for 720 h in simulated solutions with 0 g/L (a, d), 0.4 g/L (b, e) and 1 g/L (c, f) inhibitor and then removal of corrosion products