TP110TS和P110钢在CO2注入井环空环境中应力腐蚀行为比较
|
Comparison of Stress Corrosion Behavior of TP110TS and P110 Steel in a Simulated Annular Environment of CO2 Injection Well
|
图2. TP110TS和 P110钢在添加不同浓度缓蚀剂条件下浸泡720 h后的宏观形貌 |
Fig.2. Macroscopic morphologies of TP110TS (a, c) and P110 (b, d) steels after immersion for 720 h in simulated solutions without (a, b) and with 1 g/L (c, d) corrosion inhibitor |
![]() |