环氧防腐涂料在模拟海水干湿交替条件下的失效过程
|
Failure Process of Epoxy Coating Subjected Test of Alternating Immersion in Artificial Seawater and Dry in Air
|
图13. 浸泡2050 h及干湿交替210个循环后试样的微观形貌 |
Fig.13. SEM images of the coating after full immersion for 2050 h (a) and alternating wetting-drying exposure for 210 cycles (b) and the magnified images of areas I in Fig.13a (c) and III in Fig.13b (d) |
![]() |