表2 试样腐蚀产物的XRD分析结果
Table 2 Result of XRD analysis of rusted samples
MaterialCorrosion test methodMain components of corrosion product
Q235 steelField corrosion testFeOOH, Fe2O3, Fe3O4, FeS, SiO2
Accelerated corrosion testFeOOH, Fe2O3, Fe3O4, SiO2
Galvanized steelField corrosion testZnO, FeOOH, Fe2O3, SiO2
Accelerated corrosion testZnO, FeOOH, Fe2O3, SiO2
Zinc clad steelField corrosion testZn, ZnO, SiO2
Accelerated corrosion testZn, ZnO, SiO2
Zinc-magnesium alloy and copper clad steelField corrosion testZn, Zn(OH)2, MgCO3, SiO2
Accelerated corrosion testZn, Zn(OH)2, MgCO3, SiO2
CopperField corrosion testCu, CuO, Cu2O, Cu2(OH)2CO3
Accelerated corrosion testCu, CuO, Cu2O
Copper clad steelField corrosion testCu, CuO, Cu2O, Cu2(OH)2CO3
Accelerated corrosion testCu, CuO, Cu2O