红壤地区接地材料现场埋样与加速腐蚀实验的相关性研究
朱亦晨1,刘光明1(),刘欣2,裴锋2,田旭2,师超1
Investigation on Interrelation of Field Corrosion Test and Accelerated Corrosion Test of Grounding Materials in Red Soil Environment
ZHU Yichen1,LIU Guangming1(),LIU Xin2,PEI Feng2,TIAN Xu2,SHI Chao1

图5. 红壤中接地材料现场腐蚀实验296 d后的微观腐蚀形貌

Fig.5. Micro-surface morphologies of grounding materials after field corrosion test for 296 d in red soil: (a) Q235 steel, (b) galvanized steel, (c) zinc clad steel, (d) zinc-magnesium alloy and copper clad steel, (e) copper, (f) copper clad steel, (g) conductive coating clad steel, (h) stainless steel clad steel