Corten-A耐候钢在模拟污染海洋大气环境中的加速腐蚀相关性研究
冯亚丽,白子恒,陈利红,魏丹,张东玖,姚琼,吴俊升,董超芳,肖葵

Correlation of Indoor Accelerated Corrosion with Outdoor Exposure for Corten-A Weathering Steel in Polluted Marine Atmospheric Environments
Yali FENG,Ziheng BAI,Lihong CHEN,Dan WEI,Dongjiu ZHANG,Qiong YAO,Junsheng WU,Chaofang DONG,Kui XIAO
表7 万宁地区腐蚀失重的绝对差
Table 7 Absolute difference of corrosion mass loss in Wanning
Test time1%NaCl2%NaCl3.5%NaCl5%NaCl7%NaCl
Δ01Δ02Δ03Δ04Δ05
1 a (216 h)00000
2 a (432 h)0.47910.64490.68660.74750.6224
4 a (864 h)1.36351.94192.09622.32761.8604
8 a (1728 h)2.93714.45254.88045.54004.2303
12 a (2592 h)5.45486.86597.59858.74616.4894
16 a (3456 h)10.14509.206810.261711.93338.6685