工艺参数对2195铝锂合金阳极氧化膜的耐蚀性影响
肖金涛1,陈妍1,邢明秀1,鞠鹏飞1(),孟引根1,王芳2
Effect of Process Parameters on Corrosion Resistance of Anodizing Film on 2195 Al-Li Alloy
XIAO Jintao1,CHEN Yan1,XING Mingxiu1,JU Pengfei1(),MENG Yingen1,WANG Fang2

图5. 2195铝锂合金在氧化不同时间后阳极氧化膜表面形貌

Fig.5. Surface morphologies of oxide films formed on 2195 Al-Li alloy after anodization for different time: (a) 20 min, (b) 30 min, (c) 40 min, (d) 50 min