FeCr15Ni15单晶600 ℃下热生长氧化膜的TEM观察
|
TEM Investigation to Oxide Scale Formed on Single Crystal Alloy FeCr15Ni15 at High Temperature
|
图6. 氧化膜内层区域II和区域III的HAADF-STEM像 |
Fig.6. Cross-sectional HAADF-STEM images of the inner areas II and III of the oxide scale in Fig.1: (a) HAADF-STEM image of the inner area II, (b) zoom-in image showing the high resolution HAADF-STEM image of Fig.6a, (c) HAADF-STEM image of the inner area III, (d) zoom-in image showing the high resolution HAADF-STEM image of Fig.6c |
![]() |