火电厂循环泵叶轮材料Cr30A在脱硫浆液腐蚀环境中的交互损伤失效行为研究
|
Erosive Wear of Cr30A High Chromium Cast Iron in a Simulated Circulating Pump Operation Condition with Slurry Related to Wet DesulfurationProcess in Thermal Power Plant
|
图7. Cr30A铸铁在转速为1200 r/min条件下纯磨损后表面EDS分析结果 |
Fig.7. EDS result of the surface of Cr30A specimen after wear test at 1200 r/min |
![]() |