304不锈钢点蚀产物对亚稳态点蚀萌生和稳态蚀孔生长的加速作用
|
Accelerating Effect of Pitting Corrosion Products on Metastable Pitting Initiation and the Stable Pitting Growth of 304 Stainless Steel
|
图3. 亚稳态蚀孔平均峰值电流、平均峰值宽度、蚀孔数目和点蚀孕育期与转速的关系 |
Fig.3. Relationships between average peak current (a), average peak width (b), number of pits (c) and pitting incubationperiod (d) of metastable pits and stirring rate |
![]() |