304不锈钢点蚀产物对亚稳态点蚀萌生和稳态蚀孔生长的加速作用
王标,杜楠,张浩,王帅星,赵晴

Accelerating Effect of Pitting Corrosion Products on Metastable Pitting Initiation and the Stable Pitting Growth of 304 Stainless Steel
Biao WANG,Nan DU,Hao ZHANG,Shuaixing WANG,Qing ZHAO
表1 不同搅拌速度下极化后单个蚀孔的几何参数
Table 1 Geometric parameters of a single pit after polarization at different stirring rates
Stirring rate r / minD / μmd / μmH / μmV / μm3DHdH
01751031051.61×1061.670.98
10013385908.36×1051.470.94
30012579877.45×1051.430.90
5008962753.54×1051.180.82