氧化皮对SPHC热轧钢板在热带海洋大气环境中初期腐蚀行为的影响
|
Effect of Oxide Scales on Initial Corrosion Behavior of SPHC Hot Rolled Steel in Tropical Marine Atmosphere
|
图2. SPHC热轧钢板在不同暴晒周期后的表面宏观形貌 |
Fig.2. Surface macroscopic morphologies of SPHC hot rolled steel samples with (a1~a4) and without (b1~b4) oxide scales after exposure for 15 d (a1, b1), 30 d (a2, b2), 90 d (a3, b3) and 180 d (a4, b4) |
![]() |