TiAlSiN涂层对γ-TiAl基合金抗高温氧化性能的影响
|
Influence of TiAlSiN Coatings on High Temperature Oxidation Resistance of γ-TiAl Based Alloys
|
图4. TiAlSiN涂层在800 ℃下循环氧化300 h后的表面和截面形貌 |
Fig.4. Surface (a, c, e) and cross-sectional (b, d, f) morphologies of Ti0.5Al0.45Si0.05N (a, b), Ti0.5Al0.4Si0.1N (c, d) and Ti0.6Al0.3Si0.1N (e, f) coatings after cyclic oxidation at 800 ℃ for 300 h |
![]() |