稀土复合掺杂ZrO2陶瓷涂层抗Na2SO4+NaVO3热腐蚀性能的研究进展
|
Research Progress on Hot Corrosion of Rare Earth Oxides Co-doped ZrO2 Ceramic Coatings in Molten Na2SO4+NaVO3 Salts
|
图3. YSZ和CYSZ涂层在1000 ℃下Na2SO4+V2O5熔盐中分别腐蚀12和30 h后表面的XRD谱[ |
Fig.3. XRD patterns of YSZ (a) and CYSZ (b) coatings after hot corrosion in Na2SO4+V2O5 molten salt at 1000 ℃ for 12 and 30 h, respectively[ |
![]() |