核级316LN不锈钢焊接接头在高温高压水中的腐蚀性能研究
李兆登,崔振东,侯相钰,高丽丽,王维珍(),尹建华
Corrosion Property of Nuclear Grade 316LN Stainless Steel Weld Joint in High Temperature and High Pressure Water
Zhaodeng LI,Zhendong CUI,Xiangyu HOU,Lili GAO,Weizhen WANG(),Jianhua YIN

图4. 腐蚀不同时间时试样表面氧化膜典型形貌

Fig.4. SEM images of typical surface morphologies of the oxide films formed on the 316LN stainles steel weld joint after corrosion for 50 h (a), 200 h (b), 360 h (c), 760 h (d), 1080 h (e) and 1440 h (f)