管线钢的微生物腐蚀
史显波1,杨春光1,严伟1,徐大可2,闫茂成1,单以银1,杨柯1()
Microbiologically Influenced Corrosion of Pipeline Steels
Xianbo SHI1,Chunguang YANG1,Wei YAN1,Dake XU2,Maocheng YAN1,Yiyin SHAN1,Ke YANG1()

图6. 含Cu管线钢 (X80-Cu) 和X80管线钢在含有SRB的土壤浸出液中浸泡20 d后的表面腐蚀坑形貌[57]

Fig.6. Pitting morphologies of Cu-bearing (X80-Cu) (a) and X80 (b) pipeline steels after immersion for 20 d in soil-extract solution with SRB[57]