激光重熔YSZ热障涂层950 ℃的热腐蚀行为
|
|
Evaluation of Hot Corrosion Behavior of Laser As-remelted YSZ Thermal Barrier Coatings at 950 ℃
|
|
图3. 两种热障涂层热腐蚀不同时间后表面的XRD谱 |
Fig.3. XRD patterns of as-sprayed TBC (a) and as-remelted TBC (b) after hot corrosion for different time |
![]() |