激光重熔YSZ热障涂层950 ℃的热腐蚀行为
|
|
Evaluation of Hot Corrosion Behavior of Laser As-remelted YSZ Thermal Barrier Coatings at 950 ℃
|
|
图4. 喷涂态热障涂层热腐蚀不同时间后的表面微观形貌 |
Fig.4. Surface morphologies of as-sprayed TBC after hot corrosion for 10 h (a), 40 h (b) and 100 h (c) |
![]() |