304和316H不锈钢在LiF-NaF-KF熔盐中的腐蚀行为研究
|
刘辉 1,2,邱玮 1( ),冷滨 2( ),俞国军 2
|
Corrosion Behavior of 304 and 316H Stainless Steels in Molten LiF-NaF-KF
|
Hui LIU 1,2,Wei QIU 1( ),Bin LENG 2( ),Guojun YU 2
|
|
图2. 经700 ℃的FLiNaK熔盐腐蚀400 h后304和316H不锈钢的表面SEM形貌
|
Fig.2. SEM images of the surfaces of 304 (a) and 316H (b) stainless steels after corrosion at 700 ℃ in FLiNaK salt for 400 h |
|
|
|
|