几种超级不锈钢在模拟烟气脱硫环境中的缝隙腐蚀行为研究
王长罡1,魏洁1,魏欣1,穆鑫1,薛芳1,董俊华1(),柯伟1,李国平2
Crevice Corrosion Behavior of Several Super Stainless Steels in a Simulated Corrosive Environment of Flue Gas Desulfurization Process
Changgang WANG1,Jie WEI1,Xin WEI1,Xin MU1,Fang XUE1,Junhua DONG1(),Wei KE1,Guoping LI2

图2. 316,904L,254sMo和2507不锈钢的人造缝隙电极在70 ℃死亡绿液中的循环伏安曲线

Fig.2. Cyclic voltammetric curves of artificial gap electrodes of 316 (a), 904L (b), 254sMo (c) and 2507 (d) stainless steels in death green liquid at 70 ℃