高镍钢和传统耐候钢在马尔代夫严酷海洋大气环境中的腐蚀行为研究
程多云1,赵晋斌2,刘波3,姜城4,付小倩4,程学群4()
Corrosion Behavior of High Nickel and Conventional Weathering Steels Exposed to a Harsh Marine Atmospheric Environment at Maldives
Duoyun CHENG1,Jinbin ZHAO2,Bo LIU3,Cheng JIANG4,Xiaoqian FU4,Xuequn CHENG4()

图2. 室外暴晒1 a后两种钢的表面腐蚀产物微观形貌

Fig.2. Surface morphologies of corrosion products of conventional WS (a) and high nickel WS (c) after exposed for 1 a, and magnified images of the square areas in Fig.2a (b) and Fig.2c (d)