阴极面积对3.5%NaCl溶液中304不锈钢稳态点蚀生长速率的影响
|
Effect of Cathode Area on Stable Pitting Growth Rate of 304 Stainless Steel in 3.5%NaCl Solution
|
图6. 不同阴阳极面积比下动电位极化后阳极腐蚀形貌 |
Fig.6. Surface morphologies of the 304 sainless steel anode before and after potentiodynamic polarization under different conditions: (a, e) no polarization, (b, f) polarization/no additional cathode, (c, g) polarization/Sc:Sa=1, (d, h) polarization/Sc:Sa=64 |
![]() |