304L不锈钢在硝酸-硝酸钠环境中的腐蚀研究
|
Corrosion Behavior of 304L Stainless Steel in Nitric Acid-Sodium Nitrate Solutions
|
图3. 304L不锈钢在135 ℃,4% HNO3-23%NaNO3的水溶液和蒸汽中腐蚀后的截面形貌 |
Fig.3. Section micrographs of 304L stainless steel after corrosion in the solution (a) and steam (b) of 4%HNO3-23%NaNO3at 135 ℃ |
![]() |