304L不锈钢在硝酸-硝酸钠环境中的腐蚀研究
刘希武,赵小燕,崔新安(),许兰飞,李晓炜,程荣奇
Corrosion Behavior of 304L Stainless Steel in Nitric Acid-Sodium Nitrate Solutions
Xiwu LIU,Xiaoyan ZHAO,Xin'an CUI(),Lanfei XU,Xiaowei LI,Rongqi CHENG

图7. 304L不锈钢在不同温度的2%HNO3-23%NaNO3水溶液和蒸汽中腐蚀后的SEM像

Fig.7. SEM images of 304L stainless steel after corrosion in the solution (a, c) and steam (b, d) of 2% HNO3-23%NaNO3at 120 ℃ (a, b) and 135 ℃ (c, d)