304L不锈钢在硝酸-硝酸钠环境中的腐蚀研究
|
Corrosion Behavior of 304L Stainless Steel in Nitric Acid-Sodium Nitrate Solutions
|
图6. 304L不锈钢在4%HNO3-(10%,15%) NaNO3水溶液和蒸汽中腐蚀后的SEM像 |
Fig.6. SEM images of 304L stainless steel after corrosion in the solutions (a, c) and steams (b, d) of 4% HNO3-10%NaNO3(a, b) and 4%HNO3-15% NaNO3(c, d) |
![]() |