含Ag抗菌双相不锈钢表面腐蚀产物的XPS分析
刘东,向红亮,刘春育

XPS Analysis of Corrosion Product Scale on Surface of Silver-bearing Antibacterial Duplex Stainless Steel
Dong LIU,Hongliang XIANG,Chunyu LIU
表5 Mo3d5/2结合能及对应价态相对含量
Table 5 Binding energies and relative contents of Mo3d5/2
SampleTime / s228.0 eV (Mo)228.8 eV (MoCl3)229.3 eV (MoO2)230.9 eV (MoO2)231.5 eV (MoO3)232.7 eV (MoO42-)
A00.000.367.8738.3119.9033.55
1037.260.0016.9611.6720.4713.64
2081.180.0018.820.000.000.00
3083.730.0016.270.000.000.00
B00.000.976.9711.939.6470.49
1023.340.000.004.5872.080.00
2040.380.000.0059.620.000.00
3046.050.000.0053.950.000.00