表4 不同条件下钝化膜厚度与成膜电位之间的拟合曲线
Table 4 Relationships between the thickness and formation potential of the passive films under different conditions
Experimental condition Fitting equation x =0.1
Temperature 20 ℃ y =1.8836x+0.4924 y =0.6808
40 ℃ y =1.9230x+0.3765 y =0.5688
60 ℃ y =1.7752x+0.3528 y =0.5303
pH 9.27 y =3.3452x+0.9599 y =1.2944
9.78 y =3.2542x+1.2753 y =1.6007
10.84 y =3.2473x+1.5822 y =1.9069
Cl- 0.001 y =1.338x+0.1403 y =0.2741
0.003 y =0.6380x+0.1302 y =0.1940
0.005 y =0.2870x+0.1276 y =0.1563