S32750超级双相不锈钢在NaCl溶液中的临界点蚀温度及电化学腐蚀机理
|
|
何进, 晏敏胜, 杨丽景, Masoumeh Moradi, 宋振纶, 蒋业华
|
Electrochemical Corrosion and Critical Pitting Temperature of S32750 Super Duplex Stainless Steel in NaCl Solution
|
|
HE Jin, YAN Minsheng, YANG Lijing, Masoumeh Moradi, SONG Zhenlun, JIANG Yehua
|
|
| 表1 根据EIS拟合得到的各等效元件数值 |
| Table 1 Equivalent parameters obtained by fitting the EIS |
|
| Temperature / ℃ | Rs / Ωcm2 | Qpass / Ω-1sncm2 | Qpass / n1 | Rpass / Ωcm2 | Qpit / Ω-1sncm2 | Qpit / n2 | Rpit / Ωcm2 | | 25 | 3.58 | 6.16×10-5 | 0.82 | 2.50×103 | --- | --- | —— | | 35 | 2.10 | 8.23×10-5 | 0.77 | 2.06×103 | --- | --- | —— | | 45 | 2.24 | 8.88×10-5 | 0.74 | 1.99×103 | --- | --- | —— | | 55 | 1.73 | 9.59×10-5 | 0.66 | 1.97×103 | --- | --- | —— | | 65 | 1.38 | 1.06×10-4 | 0.68 | 1.94×103 | --- | --- | —— | | 75 | 2.26 | 3.92×10-5 | 0.81 | 1.24×102 | 7.03×10-5 | 0.75 | 131.50 | | 85 | 1.88 | 9.99×10-5 | 0.80 | 2.46×101 | 1.88×10-4 | 0.71 | 15.28 |
|
|
|