冷坩埚定向凝固Ti-47Al-2Cr-2Nb合金的拉伸与高周疲劳性能研究*
|
TENSILE AND HIGH CYCLE FATIGUE PROPERTIES OF Ti-47Al-2Cr-2Nb DIRECTIONALLY SOLIDIFIED BY COLD CRUCIBLE METHOD
|
图4. 抽拉速率为1.2 mm/min时定向凝固Ti-47Al-2Cr-2Nb合金中不同凝固区域的XRD谱 |
Fig.4. XRD spectra of different parts of directionally solidified Ti-47Al-2Cr-2Nb alloy at withdrawal rate of 1.2 mm/min |
![]() |