高温合金铸锭均匀化程度对开坯热变形的再结晶影响
董建新(),李林翰,李浩宇,张麦仓,姚志浩
EFFECT OF EXTENT OF HOMOGENIZATION ON THE HOT DEFORMATION RECRYSTALLIZATION OF SUPERALLOY INGOT IN COGGING PROCESS
Jianxin DONG(),Linhan LI,Haoyu LI,Maicang ZHANG,Zhihao YAO

图17. GH4738铸态合金和均匀化12 h试样经1150 ℃, 0.1 s-1, 变形量30%热变形后中心区域的FESEM像

Fig.17. FESEM images of the center area of as-cast GH4738 alloy (a) and homogenized at 1150 ℃ for 12 h after hot compression (1150 ℃, 0.1 s-1, 30%) (b)