高温合金铸锭均匀化程度对开坯热变形的再结晶影响
|
EFFECT OF EXTENT OF HOMOGENIZATION ON THE HOT DEFORMATION RECRYSTALLIZATION OF SUPERALLOY INGOT IN COGGING PROCESS
|
图7. GH4740H合金在1110 ℃下均匀化48 h后的氧化层截面形貌 |
Fig.7. Cross-sectional SEM image (a) and EDS mapping analysis of rectangular area in Fig.7a (b~d) of GH4740H alloy under homogenization at 1110 ℃ for 48 h |
![]() |