X80管线钢红壤腐蚀初期电化学行为
|
么惠平, 闫茂成, 杨旭, 孙成
|
Electrochemical Behavior of X80 Pipeline Steel in the Initial Stage of Corrosion in an Acidic Red Soil
|
YAO Huiping, YAN Maocheng, YANG Xu, SUN Cheng
|
|
表1 由等效电路 (CsRs) (QdlRct)拟合所得电化学参数 |
Table 1 Fitted EIS parameters of X80 steel in the red soil slurry |
|
Time d | Rs kΩcm2 | Cs 10-10 Fcm-2 | Rct kΩcm2 | Qdl | Y0 / S sncm-2 | n | 1 | 5.578 | 1.233 | 3.371 | 1.228×10-4 | 0.9778 | 5 | 5.365 | 0.828 | 4.052 | 1.415×10-4 | 0.8128 | 10 | 4.619 | 0.932 | 3.836 | 2.142×10-4 | 0.9458 | 15 | 3.854 | 3.825 | 3.763 | 3.069×10-4 | 0.8953 | 30 | 3.776 | 0.950 | 3.729 | 1.100×10-3 | 0.5009 | 45 | 3.605 | 1.181 | 5.729 | 1.660×10-3 | 0.4456 | 60 | 3.558 | 1.253 | 6.234 | 1.730×10-3 | 0.3957 |
|
|
|