Cr13不锈钢在盐酸溶液喷射冲刷作用下的表面腐蚀形貌表征 |
|||||||||||||||||||||
程从前, 曹铁山, 王冬颖, 姚景文, 王健, 关锰, 赵杰 | |||||||||||||||||||||
Erosion-corrosion Morphology of Cr13 Stainless Steel Induced by Jet Flow of Hydrochloric Acid Solution |
|||||||||||||||||||||
CHENG Congqian, CAO Tieshan, WANG Dongying, YAO Jingwen, WANG Jian, GUAN Meng, ZHAO Jie | |||||||||||||||||||||
表1 Cr13不锈钢不同组织的显微硬度 | |||||||||||||||||||||
Table 1 Microhardness at different microstructure zone of Cr13 stainless steel (loading force: 10 N) | |||||||||||||||||||||
|
|||||||||||||||||||||