7020铝合金在3.5%NaCl溶液中的点蚀行为
|
戴芸 1,2,3,刘胜胆 1,2,3( ),邓运来 1,2,3,张新明 1,2,3
|
Pitting Corrosion of 7020 Aluminum Alloy in 3.5%NaCl Solution
|
Yun DAI 1,2,3,Shengdan LIU 1,2,3( ),Yunlai DENG 1,2,3,Xinming ZHANG 1,2,3
|
|
图7. 7020铝合金浸泡不同时间后的SEM像和EDS分析结果
|
Fig.7. SEM images (a, c) and EDS results (b, d) of 7020 aluminum alloy after immersion for 168 h (a, b) and 1176 h (c, d) |
|
|
|
|