铝合金阳极氧化层在江津污染大气环境中暴露腐蚀行为研究
周和荣(),胡碧华,姚望,洪新培,宋述鹏
Atmospheric Corrosion of Anodized Pure Al 1060, Al-alloys 2A12 and 7A04 Exposed to Polluted Atmospheric Environment at Jiangjin Region
Herong ZHOU(),Bihua HU,Wang YAO,Xinpei HONG,Shupeng SONG

图4. 图3f中1-2位置处腐蚀产物的EDS分析

Fig.4. EDS line-scanning results from point 1 to point 2 in Fig.3f: (a) O, (b) Al, (c) Si and (d) S