WMCNTs/AZ31复合材料电化学腐蚀研究
周国华1,2
1. 宜春学院物理科学与工程学院 宜春 336000;
2. 北京科技大学新金属材料国家重点实验室 北京 100083
Electrochemical Corrosion of MWCNTs/AZ31 Composite
ZHOU Guohua1,2
1. Physical Science and Technology College, Yichun University, Yichun 336000, China;
2. State Key Laboratory for Advanced Metals and Materials, Univerty of Science and Technology Beijing, Beijing 100083, China
全文: PDF(3868 KB)  
摘要: 采用碳纳米管孕育块铸造法制备碳纳米管/AZ31镁基复合材料,测量其电化学极化曲线,研究碳纳米管加入量对复合材料抗腐蚀性能的影响,利用SEM对复合材料腐蚀前后的表面形貌进行了观察和分析。结果表明,碳纳米管的加入有效地提高了复合材料的抗腐蚀性能,随着复合材料中碳纳米管加入量的增加,腐蚀电流密度Icorr由5.279 μA/cm2减小到2.994 μA/cm2
关键词 碳纳米管AZ31镁合金复合材料腐蚀    
Abstract:Multi-walled carbon nonotubes (MWCNTs) /AZ31 composites were fabricated by joining preform of MWCNTs during melting. The corrosion behaviors of the composites were studied by electrochemical corrosion experiments in 3.5% (mass fraction) NaCl solution. The surface morphologies of the composites before and after corrosion were observed and analysised by SEM. The results showed that additions of MWCNTs improved anticorrosive performances of AZ31 Mg-based alloy, the corrosion current density (Icorr) decreased from 5.279 to 2.994 μA/cm2.
Key wordsmulti-walled carbon nonotubes (MWCNTs)    AZ31 magnesium alloy    composite   
corrosion
    
ZTFLH:  TB333  

引用本文:

周国华. WMCNTs/AZ31复合材料电化学腐蚀研究[J]. 中国腐蚀与防护学报, 2013, 33(5): 430-434.
ZHOU Guohua. Electrochemical Corrosion of MWCNTs/AZ31 Composite. Journal of Chinese Society for Corrosion and protection, 2013, 33(5): 430-434.

链接本文:

https://www.jcscp.org/CN/      或      https://www.jcscp.org/CN/Y2013/V33/I5/430

[1] Yu K, Li W X, Wang R C, et al. Research, development and application of wrought magnesium alloys [J]. Chin. J. Nonferrous Met., 2003, 13(2): 277-287
(余琨, 黎文献, 王日初等. 变形镁合金的研究、开发及应用 [J]. 中国有色金属学报, 2003, 13(2): 277-287)
[2] Gu C D, Lian J S, Li G Y, et al. Electroless Ni-P plating on the AZ91D magnesium alloy [J]. J. Chin. Soc. Corros. Prot., 2005, 25(5): 271-274
(谷长栋, 连建设, 李光玉等. AZ91D镁合金的化学镀镍 [J]. 中国腐蚀与防护学报, 2005, 25(5): 271-274)
[3] Kwo Z C, Teng S S. Conversion-coating treatment for magnesium alloys by a permanganate phosphate solution [J]. Mater. Chem. Phys., 2003, 80(1): 191-200
[4] Almeida E. Surface treatments and coatings for metals a general overview [J]. Ind. Eng. Chem. Res., 2001, 40(1): 3-14
[5] Hoche H, Rosenkranz C, Delp A, et al. Investigation of the macroscopic and microscopic electrochemical corrosion behavior of PVD-coated magnesium die cast alloy AZ91 [J]. Surf. Coat. Technol., 2005, 10(3): 178-184
[6] Wu G S, Zeng X Q, Li G Y, et al. Preparation and characterization of ceramic/metal duplex coations deposited on AZ31 magnesium alloy by multi-magnetron sputting [J]. Mater. Lett., 2006, 60(5): 674-678
[7] Wu C S. Study on the anodizing and corrosion behavior of AZ31 magnesium alloys [D]. Hangzhou: Zhejiang University, 2006
(吴昌胜. AZ31镁合金阳极氧化工艺及腐蚀行为研究 [D]. 杭州: 浙江大学, 2006)
[8] Zhi Q, Gao J, Dong C F, et al. Corrosion behavior of microarc oxidation film on AZ91D magnesium alloy [J]. Acta Metall. Sin., 2008, 44(8): 986-990
(郅青, 高瑾, 董超芳等. AZ91D镁合金微弧氧化膜的腐蚀行为研究 [J]. 金属学报, 2008, 44(8): 986-990)
[9] Zhou G H, Zeng X S, Yuan Q H. Study on carbon nanotubes/AM60 magnesium matrix composites by cast [J]. Foundry, 2009, 58(1): 43-46
(周国华, 曾效舒, 袁秋红. 铸造法制备CNTs/AM60镁基复合材料的研究 [J]. 铸造, 2009, 58(1): 43-46)
[10] Thakur S K, Srivatsan T S. Synthesis and mechanical behavior of carbon nanotube-magnesium composites hybridized with nanoparticles of alumina [J]. Mater. Sci. Eng., 2007, A466(1): 32-37
[11] Endo M, Hayashi T, Ltoh L, et al. An anticorrosive magnesium/carbon nanotube composite [J]. Appl. Phys. Lett., 2008, 92(6): 1-3
[12] Montemor M F, Ferreira M G S. Analytical characterization and corrosion behaviour of bis-aminosilance modified with carbon nanotubes activated with rare-earth salts applied on AZ31 magnesium alloy [J]. Surf. Coat. Technol., 2008, 202(1): 4766-4774
[13] Liu D X. Corrosion and Protection of Materials [M]. Xi'an: Northwest Industrial University Press, 2005
(刘道新. 材料的腐蚀与防护 [M]. 西安: 西北工业大学出版社, 2005)
[14] Zhou G H. The Research of MWCNTs/AZ31 magnesium matrix composites and equal channel angular pressing [D]. Nanchang: Nanchang University, 2010
(周国华. 碳纳米管/AZ31镁基复合材料的制备与等径角挤压研究 [D]. 南昌: 南昌大学, 2010)
[15] Zhou G H, Zeng X S, Xu Q. Microstructure evolution and mechanical behavior of CNTs/AZ31 magnesium alloy composites processed by equal channel angular pressing [J]. Adv. Mater. Res., 2010, 97(101): 1628-1632
[16] Yin D S, Zhang E L, Zeng S Y. Effcet of extrusion on mechanical properties and corrosion behavior of Mg-Mn-Zn alloy [J]. Trans. Mater. Heat Treat., 2009, 30(1): 114-118
(尹冬松, 张二林, 曾松岩. 挤压对Mg-Mn-Zn合金力学性能和腐蚀行为的影响 [J]. 材料热处理学报, 2009, 30(1): 114-118)
[17] Wu L J. The effect of hot extrusion on corrosion behavior of AZ91 magnesium alloy and SiCp/AZ91 composite [D]. Harbin: Harbin Institute of Technology, 2007
(吴丽娟. 热挤压对AZ91镁合金和SiCp/AZ91复合材料腐蚀行为的影响 [D]. 哈尔滨: 哈尔滨工业大学, 2007)
[1] 董续成, 管方, 徐利婷, 段继周, 侯保荣. 海洋环境硫酸盐还原菌对金属材料腐蚀机理的研究进展[J]. 中国腐蚀与防护学报, 2021, 41(1): 1-12.
[2] 唐荣茂, 朱亦晨, 刘光明, 刘永强, 刘欣, 裴锋. Q235钢/导电混凝土在3种典型土壤环境中腐蚀的灰色关联度分析[J]. 中国腐蚀与防护学报, 2021, 41(1): 110-116.
[3] 韩月桐, 张鹏超, 史杰夫, 李婷, 孙俊才. 质子交换膜燃料电池中TA1双极板的表面改性研究[J]. 中国腐蚀与防护学报, 2021, 41(1): 125-130.
[4] 张雨轩, 陈翠颖, 刘宏伟, 李伟华. 铝合金霉菌腐蚀研究进展[J]. 中国腐蚀与防护学报, 2021, 41(1): 13-21.
[5] 冉斗, 孟惠民, 刘星, 李全德, 巩秀芳, 倪荣, 姜英, 龚显龙, 戴君, 隆彬. pH对14Cr12Ni3WMoV不锈钢在含氯溶液中腐蚀行为的影响[J]. 中国腐蚀与防护学报, 2021, 41(1): 51-59.
[6] 左勇, 曹明鹏, 申淼, 杨新梅. MgCl2-NaCl-KCl熔盐体系中金属Mg对316H不锈钢的缓蚀性能研究[J]. 中国腐蚀与防护学报, 2021, 41(1): 80-86.
[7] 王欣彤, 陈旭, 韩镇泽, 李承媛, 王岐山. 硫酸盐还原菌作用下2205双相不锈钢在3.5%NaCl溶液中应力腐蚀开裂行为研究[J]. 中国腐蚀与防护学报, 2021, 41(1): 43-50.
[8] 史昆玉, 吴伟进, 张毅, 万毅, 于传浩. TC4表面沉积Nb涂层在模拟体液环境下的电化学性能研究[J]. 中国腐蚀与防护学报, 2021, 41(1): 71-79.
[9] 郑黎, 王美婷, 于宝义. 镁合金表面冷喷涂技术研究进展[J]. 中国腐蚀与防护学报, 2021, 41(1): 22-28.
[10] 于宏飞, 邵博, 张悦, 杨延格. 2A12铝合金锆基转化膜的制备及性能研究[J]. 中国腐蚀与防护学报, 2021, 41(1): 101-109.
[11] 贾世超, 高佳祺, 郭浩, 王超, 陈杨杨, 李旗, 田一梅. 再生水水质因素对铸铁管道的腐蚀研究[J]. 中国腐蚀与防护学报, 2020, 40(6): 569-576.
[12] 赵鹏雄, 武玮, 淡勇. 空间分辨技术在金属腐蚀原位监测中的应用[J]. 中国腐蚀与防护学报, 2020, 40(6): 495-507.
[13] 马鸣蔚, 赵志浩, 荆思文, 于文峰, 谷义恩, 王旭, 吴明. 17-4 PH不锈钢在含SRB的模拟海水中的应力腐蚀开裂行为研究[J]. 中国腐蚀与防护学报, 2020, 40(6): 523-528.
[14] 岳亮亮, 马保吉. 超声表面滚压对AZ31B镁合金腐蚀行为的影响[J]. 中国腐蚀与防护学报, 2020, 40(6): 560-568.
[15] 艾芳芳, 陈义庆, 钟彬, 李琳, 高鹏, 伞宏宇, 苏显栋. T95油井管在酸性油气田环境中的应力腐蚀开裂行为及机制[J]. 中国腐蚀与防护学报, 2020, 40(5): 469-473.